← Back to Articles

What a Complete Mold Quote Includes (Chinese Industry Standard)

July 11, 2026

What a Complete Mold Quote Includes (Chinese Industry Standard)

Decoding a Chinese Mold Quote

A professional Chinese mold quote should include transparent cost breakdowns. Here is what to expect — and what to watch for.

What Should Be Included

  • Material Cost (30-40%): Steel for cavity, core, and mold base. Should specify steel grade, supplier, and estimated weight.
  • Machining Cost (35-45%): CNC roughing, finishing, EDM, wire cutting, grinding. More complex dies have higher machining ratios.
  • Design Cost (5-10%): 3D modeling, DFM analysis, cooling analysis. Good factories include 2-3 design iterations.
  • Assembly & Testing (5-8%): Fit-up, hot runner wiring, mold tryout.
  • Profit Margin (10-20%): Standard industry range.
  • Tax (VAT 13%): Domestic Chinese VAT. Export orders may be VAT-exempt with proper documentation.

What Is Typically Extra

  • Hot Runner System: Usually priced separately ($500-5,000 depending on brand and number of drops)
  • Mold Trial Shots: First round often included, additional rounds charged at press time + material cost
  • Design Changes After DFM Approval: Revisions after sign-off are typically billed at hourly rates
  • Shipping and Logistics: Usually quoted separately unless DDP terms agreed
  • Special Surface Treatment: Nitriding, PVD coating, chrome plating

How to Compare Quotes Effectively

When comparing quotes from different factories:

  • Normalize for scope: Ensure all quotes include the same items
  • Check steel grade consistency: One factory quoting P20 vs another quoting 718H is not apples-to-apples
  • Look at the total, not the breakdown: Individual line items can vary wildly, but total cost for similar specifications should be within 15-20%
  • Beware the "lowball" quote: If one factory is 40% cheaper, they are cutting corners somewhere

Use our online quoting tool to get a reference price before requesting formal quotes from factories.